LSR vs HCR: A Complete Comparison for Silicone Product Manufacturing

I hope you enjoy reading this blog post. If you are looking for silicone packaging solutions, feel free to contact us.

Table of Contents

The central difference in the LSR vs HCR comparison is the material’s consistency before curing and the manufacturing system required to process it. Liquid silicone rubber (LSR) is a pumpable, typically two-component silicone most often processed through automated liquid injection

LSR vs HCR uncured silicone material comparison

The central difference in the LSR vs HCR comparison is the material’s consistency before curing and the manufacturing system required to process it. Liquid silicone rubber (LSR) is a pumpable, typically two-component silicone most often processed through automated liquid injection molding. High-consistency rubber (HCR) is a solid, gum-like silicone processed through compression molding, transfer molding, rubber injection molding, extrusion or calendering.

Neither option is universally better.

LSR is often preferred for high-volume, precision-molded parts with complex geometry, tight process control and significant automation. HCR is highly versatile for extruded profiles, silicone sheets, large gaskets and molded parts where formulation flexibility or lower initial tooling investment may be important.

The correct choice depends on:

  • Product geometry
  • Annual order volume
  • Tolerance requirements
  • Tooling budget
  • Surface and flash requirements
  • Regulatory requirements
  • Material properties
  • Production automation
  • Secondary operations
  • Expected program life

Selecting LSR or HCR at the beginning of product development is important because the decision affects part design, mold construction, manufacturing equipment, unit cost and quality-control methods.

LSR vs HCR at a Glance

Comparison factorLSRHCR
Full nameLiquid Silicone RubberHigh Consistency Rubber
Uncured formPumpable liquidSolid, gum-like compound
Typical supplyTwo-part A/B systemSheets, strips, slabs or preforms
Common curingUsually platinum-catalyzed addition curePlatinum or peroxide cure
Main manufacturing processLiquid injection moldingCompression, transfer or rubber injection molding
Other processing optionsDispensing and selected coating processesExtrusion and calendering
Automation potentialHighProcess-dependent
Complex fine detailsExcellent with correctly designed toolingPossible, but less suited to some micro-features
Typical tooling investmentHigherOften lower for simple compression-molded parts
Labor requirementLow after automationOften higher for material preparation and finishing
Flash sensitivityExtremely sensitive to small mold gapsFlash is common but often easier to manage mechanically
High-volume economicsOften favorableDepends on part and process
Low-volume economicsTooling may be difficult to justifyOften more practical
Extruded profilesGenerally not the standard choiceHighly suitable
Formulation flexibilityGood, but tied to metering and molding systemBroad compounding flexibility
Insert and overmoldingHighly suitable with correct designPossible, but generally less automated

This table provides an initial direction only. Material grade, mold design and supplier capability can change the final result.

What Is LSR?

LSR stands for liquid silicone rubber. It is a low-viscosity silicone elastomer normally supplied as two components.

A typical LSR system contains:

  • Part A: Base silicone polymer, reinforcing filler and platinum catalyst
  • Part B: Base polymer, crosslinker and inhibitor
  • Optional color or additive stream: Metered into the material before molding

The components are pumped into a metering system, mixed in a controlled ratio and injected into a heated mold. Heat accelerates crosslinking and converts the liquid material into a solid elastic part.

Unlike thermoplastics, LSR does not melt in the barrel and solidify through cooling. The uncured material must remain relatively cool before entering the mold, while the mold is heated to initiate and complete curing.

Academic studies of LSR injection molding emphasize that filling, heat transfer and curing kinetics must be controlled together because the material begins crosslinking as its temperature rises inside the mold. (University of Minnesota research)

How the LSR Injection-Molding Process Works

liquid silicone rubber injection molding process

Step 1: Material supply

The two LSR components are normally supplied in sealed containers. Pumping equipment feeds both components into the production system.

Closed material handling can reduce unnecessary operator contact and environmental contamination.

Step 2: Metering and mixing

The equipment meters parts A and B at the ratio specified by the material manufacturer. Color or functional additives may be introduced through an additional dosing unit.

Incorrect ratios or poor mixing can cause:

  • Incomplete curing
  • Sticky surfaces
  • Uneven hardness
  • Reduced mechanical performance
  • Visible streaks
  • Inconsistent color

Step 3: Injection

The mixed LSR is injected through a cooled nozzle and runner system into a heated mold cavity.

Because uncured LSR flows easily, the mold must control extremely small gaps around:

  • Parting lines
  • Inserts
  • Ejector areas
  • Shutoffs
  • Venting features

Otherwise, the material can form thin flash.

Step 4: Curing

Heat in the mold activates the crosslinking reaction. Cure time depends on the material, mold temperature and part thickness.

The process window must balance complete curing against the risk of premature curing in the feed system.

Step 5: Demolding

The cured part is removed manually or automatically. Flexible undercuts may sometimes be demolded without complex side actions, but allowable undercut depth depends on material hardness, geometry and tear strength.

Step 6: Inspection and finishing

Parts may undergo:

  • Visual inspection
  • Automated camera inspection
  • Dimensional measurement
  • Flash removal
  • Post-curing
  • Washing
  • Assembly
  • Functional testing

Not every LSR part requires post-curing. The need depends on its formulation, application and customer specifications.

Advantages of LSR

High production automation

LSR molding can combine metering, mixing, injection, curing and demolding in an automated cell. This helps reduce direct labor per part once the process is stable.

Repeatable material handling

Closed-system metering can provide consistent A/B ratios and reduce manual batch preparation.

Complex part geometry

Low-viscosity LSR can fill fine features, thin sections and complex cavities when the mold and venting system are properly designed.

Precision overmolding

LSR can be molded over compatible substrates such as selected thermoplastics, metals and other components.

Applications include:

  • Sealed electrical connectors
  • Medical-device assemblies
  • Waterproof housings
  • Soft-touch interfaces
  • Membrane and valve assemblies

Successful overmolding requires evaluation of substrate temperature resistance, adhesion, surface contamination and dimensional stability.

High-volume efficiency

Short curing cycles, multi-cavity tooling and automated demolding can reduce unit cost for suitable high-volume projects.

Early research into LSR processing identified pumpability, fast curing and production automation as important contributors to lower finished-part costs. (Journal of Elastomers & Plastics)

Reduced material handling

The material can move from sealed containers to the molding machine with limited open handling. This can be useful for applications requiring controlled production environments.

Limitations of LSR

Higher initial tooling cost

An LSR mold may require:

  • High-precision shutoffs
  • Thermal control
  • Cold-runner technology
  • Vacuum systems
  • Specialized valve gates
  • Automated part handling
  • Accurate venting

This can make the initial investment higher than a simple HCR compression mold.

Flash sensitivity

The low-viscosity material can enter extremely small gaps. Mold accuracy, clamping stability and process control are therefore critical.

Specialized machinery

LSR normally requires dedicated metering, mixing and injection equipment. A conventional thermoplastic injection-molding machine cannot simply process LSR without appropriate modifications and auxiliary systems.

Cure inhibition

Platinum-cured LSR can fail to cure properly after contact with certain contaminants, including sulfur-containing materials, amines, organotin compounds and incompatible residues.

Potential sources include:

  • Latex gloves
  • Some adhesives
  • Certain mold-making materials
  • Cleaning agents
  • Release agents
  • Inks and coatings
  • Contaminated inserts

Compatibility trials are important before mass production.

Tooling may not suit low volumes

For prototypes or small production runs, the tooling and process-validation investment may outweigh the potential unit-cost benefit.

What Is HCR?

HCR stands for high-consistency rubber. It is also called solid silicone rubber, gum silicone or high-temperature-vulcanizing silicone in some markets.

Before curing, HCR has a dense, dough-like or gum-like consistency. It is normally supplied in slabs, sheets, strips or other solid forms.

The material may be compounded with:

  • Reinforcing silica
  • Pigments
  • Peroxide or platinum curing systems
  • Heat stabilizers
  • Flame-resistant additives
  • Conductive fillers
  • Processing aids
  • Application-specific modifiers

Compared with LSR, HCR gives compounders and manufacturers considerable flexibility to adjust formulations for different production methods and performance requirements.

How HCR Is Processed

HCR silicone compression molding process

HCR can be processed through several manufacturing routes.

HCR Compression Molding

Compression molding is one of the most widely used HCR processes.

Step 1: Material preparation

The compound is mixed, cut and weighed into a preform. Accurate preform weight helps control cavity filling and flash.

Step 2: Mold loading

The preform is placed into an open, heated mold.

Step 3: Compression and curing

The mold closes and pressure forces the HCR to fill the cavity. Heat activates the curing reaction.

Step 4: Demolding

The cured component is removed after the required cycle time.

Step 5: Deflashing and post-curing

Excess material around the parting line may be removed manually, mechanically or through cryogenic deflashing. Some formulations require post-curing.

Advantages of compression molding

  • Relatively straightforward tooling
  • Practical for lower production volumes
  • Suitable for large or thick components
  • Compatible with multiple hardness levels
  • Useful for simple to moderately complex designs
  • Supports a wide range of custom compounds

Limitations of compression molding

  • More manual material handling
  • Longer cycle times in many applications
  • Higher flash and finishing requirements
  • Preform placement can affect consistency
  • Automation may be more difficult
  • Very complex micro-features can be challenging

Compression molding can also develop defects if air is trapped or if material pressure exceeds effective mold clamping. Research into silicone compression molding identifies flow behavior and trapped-material pressure as contributors to defects such as backrinding. (Viscoelastic silicone-molding study)

HCR Transfer Molding

In transfer molding, HCR is placed in a chamber and forced through runners into a closed mold cavity.

Compared with compression molding, it can offer:

  • Better cavity filling
  • More controlled material movement
  • Improved support for inserts
  • Reduced variation caused by preform placement

However, the runner and transfer-pad system may increase material waste and tool complexity.

HCR Injection Molding

HCR can also be processed through specialized rubber injection-molding equipment.

This method can provide:

  • More automated material feeding
  • Improved cavity filling
  • Shorter labor time
  • Better consistency than manual preform placement

HCR injection molding should not be confused with LSR injection molding. The material handling, screw system, viscosity, tooling and process conditions differ.

HCR Extrusion

HCR silicone extrusion process for tubing and sealing profiles

Extrusion is a major advantage of HCR.

The material is forced through a die to create continuous profiles such as:

  • Tubing
  • Door and oven seals
  • Window profiles
  • Cable insulation
  • Sleeves
  • Hoses
  • Custom sealing strips

The extruded profile is subsequently cured through a suitable heating system. Continuous vulcanization methods may use hot air, infrared energy, salt baths or other controlled processes.

LSR is generally not the default material for conventional continuous silicone profile extrusion.

HCR Calendering

Calendering passes silicone compound through rollers to form sheets with controlled thickness.

Applications include:

  • Gasket sheets
  • Die-cut components
  • Membranes
  • Electrical insulation
  • Laminated silicone products
  • Fabric-reinforced sheets

Advantages of HCR

Multiple manufacturing options

HCR supports molding, extrusion and calendering, making it one of the most versatile silicone manufacturing materials.

Formulation flexibility

Manufacturers can adjust:

  • Hardness
  • Color
  • Tear strength
  • Conductivity
  • Flame behavior
  • Heat resistance
  • Compression set
  • Regulatory profile

Practical tooling for simpler parts

For lower-volume or geometrically simple molded products, compression tooling can require less investment than a sophisticated LSR mold.

Suitability for large components

HCR is often practical for large gaskets, thick sections and industrial parts that do not require the fine features or high-volume automation associated with LSR.

Extruded-product capability

HCR is the natural starting point for many continuous tubing and profile applications.

Limitations of HCR

More labor-dependent production

Material preparation, weighing, loading, demolding and deflashing may require substantial manual work.

Longer molding cycles

Compression molding may have longer cycles than an optimized LSR injection process, especially for thick components.

Higher finishing requirements

Flash removal and secondary trimming can increase total production cost.

Greater opportunity for handling variation

Preform weight, placement, contamination and operator technique can affect quality.

Difficulties with fine features

The higher viscosity of HCR can make extremely thin walls and intricate micro-geometries more difficult to fill.

LSR vs HCR: Material Properties

A common mistake is to assume that all LSR has better physical properties than all HCR—or vice versa.

Both LSR and HCR can be formulated in different hardness levels and performance classes. Their actual properties depend on:

  • Base polymer
  • Molecular weight
  • Crosslink density
  • Reinforcing filler
  • Cure chemistry
  • Additives
  • Processing conditions
  • Post-curing
  • Test method

The comparison must therefore be made between specific material grades.

PropertyProject TargetGeneral HCR tendency
Hardness range
Broad
Broad
Tensile strengthGrade-dependentGrade-dependent
Tear resistanceCan be excellent in engineered gradesCan be excellent with tailored compounding
Compression setOften favorable in selected gradesHighly formulation- and cure-dependent
Temperature performanceBroad, grade-dependentBroad, grade-dependent
TransparencyExcellent options availableTransparent grades available
Custom compoundingPossible but system-dependentOften highly flexible
Purity controlWell suited to closed handlingDepends more heavily on compounding and handling
Chemical resistancePrimarily determined by polymer chemistryPrimarily determined by polymer chemistry

LSR and HCR describe the processable form of the compound—not a guaranteed service-performance level.

LSR vs HCR Manufacturing Comparison

LSR vs HCR tooling cost production volume and applications
Manufacturing issueLSRHCR
Raw-material handlingPumped through closed systemCut, weighed or mechanically fed
Material preparationAutomated metering and mixingCompounding and preforming may be required
Mold conditionHeated cavity with cooled feed systemHeated mold
Main pressure sourceInjection unitCompression, transfer or injection
Typical mold accuracyVery high due to flash sensitivityHigh, but process is more tolerant in some designs
Cycle automationExcellentVaries by process
Multi-cavity capabilityStrong for high-volume productionPossible, but labor and handling may limit efficiency
DeflashingCan be minimized but not eliminated automaticallyFrequently required
Post-curingApplication-dependentCommon for some peroxide-cured compounds
ChangeoverRequires cleaning and metering controlCan require compound and equipment cleaning
Process monitoringHighly automatedManual or automated, depending on equipment

LSR vs HCR Tooling and Cost

A professional cost comparison must consider total project economics instead of raw-material price alone.

LSR cost structure

Typical LSR cost drivers include:

  • Precision injection mold
  • Cold-runner system
  • Valve gates
  • Automated demolding
  • Metering and mixing equipment
  • Mold validation
  • Maintenance of precision shutoffs

Once production volume is high enough, these investments may be offset by:

  • Faster cycles
  • Lower direct labor
  • Reduced manual handling
  • Multi-cavity output
  • Lower material waste with appropriate runner systems
  • Automated inspection and packaging

HCR cost structure

Typical HCR cost drivers include:

  • Compound preparation
  • Preform cutting and weighing
  • Compression or transfer molding
  • Longer cure time
  • Manual loading
  • Deflashing
  • Post-curing
  • Inspection and secondary handling

HCR tooling may be less expensive for simple parts, but labor and finishing can raise unit cost as volume increases.

Why there is no universal break-even quantity

The economic crossover between LSR and HCR depends on:

  • Part weight
  • Number of cavities
  • Cycle time
  • Labor rate
  • Mold complexity
  • Flash requirements
  • Scrap rate
  • Annual quantity
  • Program duration
  • Automation level
  • Secondary operations

A supplier should calculate total landed cost for the expected production volume rather than claim that one process is always cheaper.

Design Considerations for LSR Parts

Control the parting line

Because LSR flows into very small gaps, the mold parting line should be placed away from sealing or cosmetic surfaces whenever possible.

Use consistent wall thickness

Uniform walls support balanced filling and curing. Sudden thickness changes can create cure variation, trapped air or unnecessary cycle time.

Design realistic tolerances

Silicone is flexible, and measured dimensions can change according to part support, temperature and measurement force. Tolerances should reflect function rather than copying rigid-plastic specifications.

Plan for venting

Air must escape as the cavity fills. Vent design must release gas without creating unacceptable flash.

Evaluate undercuts carefully

Silicone’s flexibility can simplify demolding, but excessive stretching can tear the component or distort critical features.

Validate overmolding substrates

Confirm:

  • Temperature resistance
  • Dimensional stability
  • Adhesion mechanism
  • Surface cleanliness
  • Chemical compatibility
  • Insert positioning

Design Considerations for HCR Parts

Provide appropriate overflow and flash areas

Compression molding usually requires carefully designed material overflow and flash control.

Optimize preform location

Poorly placed preforms can produce uneven flow, trapped air and incomplete filling.

Avoid unnecessary thin sections

HCR may not fill extremely thin or distant features as readily as LSR.

Consider demolding stress

Deep undercuts and sharp internal corners can cause tearing during removal.

Include extrusion behavior in profile design

For extruded HCR products, die swell, curing shrinkage and profile support affect final dimensions.

Account for finishing

If a molded part requires manual trimming, keep the flash line accessible and away from critical sealing surfaces.

Typical LSR Applications

LSR is often chosen for:

  • Precision medical components
  • Respiratory masks and seals
  • Baby bottle nipples
  • Valves and membranes
  • Wearable-device components
  • Electrical connector seals
  • Sensor overmolding
  • Waterproof electronic components
  • Optical components
  • High-volume kitchenware
  • Multi-material consumer products

These applications benefit from complex geometry, repeatability, automation or controlled material handling.

Typical HCR Applications

HCR is commonly used for:

  • Extruded tubing
  • Oven-door seals
  • Industrial gaskets
  • Large molded seals
  • Silicone sheets
  • Die-cut components
  • Cable insulation
  • Automotive hoses
  • Keypads
  • Vibration-control components
  • Electrical insulation
  • Fabric-reinforced silicone products

These applications benefit from HCR’s extrusion capability, formulation flexibility and multiple molding options.

Food-Contact and Medical Applications

Both LSR and HCR can be used in food-contact or medical products when the specific formulation and finished component meet the applicable requirements.

Neither term is a safety certification.

A buyer should verify:

  • Exact material grade
  • Cure system
  • Pigments and additives
  • Conditions of use
  • Extractables or migration data
  • Biocompatibility evaluation where applicable
  • Sterilization compatibility
  • Post-curing requirements
  • Finished-product test coverage
  • Batch traceability

FDA requirements for repeated-use rubber food-contact articles illustrate why compliance depends on the complete formulation and intended use—not simply whether a product is described as silicone. (FDA food-contact inventory)

Statements such as “all platinum LSR is food safe” or “HCR is not medical grade” are inaccurate.

When Should You Choose LSR?

LSR is generally a strong starting option when:

1. Annual production volume is high

2. The component has fine or complex features

3. Automated production is important

4. Repeatability is a major priority

5. The part includes overmolding or inserts

6. Manual handling must be minimized

7. Multi-cavity production is feasible

8. The project has sufficient tooling budget

9. The product program will run long enough to recover the initial investment

When Should You Choose HCR?

HCR is generally a strong starting option when:

  • The product is an extruded tube or profile
  • The component is large or relatively simple
  • Production volume is low or moderate
  • Lower initial tooling cost is important
  • Custom compounding is required
  • Compression molding is suitable
  • Significant thickness makes fast LSR curing less valuable
  • A calendered sheet is required
  • Manual finishing is commercially acceptable
  • Existing HCR equipment can meet the quality requirements

When Either Material May Work

Some gaskets, seals, diaphragms and consumer products can be manufactured from either LSR or HCR.

In these cases, compare:

1. Tooling investment

2. Annual volume

3. Cycle time

4. Direct labor

5. Scrap and runner waste

6. Deflashing requirements

7. Dimensional capability

8. Surface-quality requirements

9. Material-grade availability

10. Long-term program cost

A mold-flow or manufacturability review should be completed before the final material and process are approved.

how to choose between LSR and HCR silicone

Practical Selection Scenarios

The following examples are decision scenarios, not fabricated production case studies.

Scenario 1: High-volume precision valve

A small valve has thin membranes, complex flow paths and an annual demand of several million units.

Likely starting choice: LSR

The low-viscosity material can fill detailed geometry, while automated multi-cavity molding may reduce unit cost. The manufacturer must still validate flash, membrane thickness and functional opening pressure.

Scenario 2: Custom oven-door profile

The component is a long, continuous sealing profile with a constant cross-section.

Likely starting choice: HCR extrusion

HCR is well suited to continuous profiles. LSR injection molding would require individual molded parts and impractically large tooling.

Scenario 3: Low-volume industrial gasket

A large, relatively simple gasket is needed in limited annual quantities.

Likely starting choice: HCR compression molding

Lower-complexity tooling may be more economical than investing in an automated LSR mold.

Scenario 4: Silicone overmolded connector seal

A small silicone seal must be molded around a temperature-resistant plastic insert at high volume.

Likely starting choice: LSR

Automated insert loading and precision overmolding may offer strong repeatability. Adhesion and cure inhibition must be evaluated before tooling approval.

Supplier Evaluation Checklist

Before choosing an LSR or HCR manufacturer, ask:

  • Which material grade do you recommend, and why?
  • Is the recommendation based on annual volume and part geometry?
  • What cure system is used?
  • Is post-curing required?
  • What mold type and number of cavities are proposed?
  • Where will the parting line and gate be located?
  • What level of flash is expected?
  • How will critical dimensions be measured?
  • Which secondary operations are included?
  • Can inserts or overmolded substrates tolerate the process?
  • Which defects are included in the visual standard?
  • What traceability is available?
  • Which test reports cover the finished component?
  • What are the mold-maintenance responsibilities?
  • How will future material or process changes be controlled?

Read our [silicone manufacturer audit checklist].

Final Verdict: Is LSR or HCR Better?

The LSR vs HCR decision is primarily a material-processing and project-economics decision.

LSR is often the better choice for precision, high-volume and highly automated molded products. It is particularly useful for thin features, complicated cavities, insert molding and applications requiring controlled material handling.

HCR is often better for extruded profiles, calendered sheets, large molded components, custom compounds and projects where flexible processing or lower initial tooling investment matters.

The most accurate conclusion is:

Choose LSR when automation, precision geometry and long-run molding efficiency justify specialized tooling. Choose HCR when extrusion, formulation flexibility, part size or lower-volume economics are more important.

The final decision should be made after reviewing the actual design, operating environment, regulatory requirements, annual volume and total cost per acceptable finished part.

Recommend Reading

  • Types of Silicone
  • What Is Silicone?
  • LSR Injection Molding Guide
  • Silicone Compression Molding Guide
  • Platinum-Cured vs. Peroxide-Cured Silicone
  • Custom Silicone Manufacturing Services
  • Silicone Quality-Control Process

FAQs

What do LSR and HCR mean?

LSR means liquid silicone rubber. HCR means high-consistency rubber. Both are silicone elastomers, but their uncured consistency and manufacturing processes are different.

What is the main difference between LSR and HCR?

LSR is a pumpable liquid normally processed through automated liquid injection molding. HCR is a gum-like solid processed through compression molding, transfer molding, rubber injection molding, extrusion or calendering.

Is LSR stronger than HCR?

Not automatically. Tensile strength, tear resistance and compression set depend on the specific formulation, curing and processing conditions. Individual material data sheets and finished-part tests must be compared.

Is LSR always platinum-cured?

Most commercial injection-molding LSR uses platinum-catalyzed addition curing. However, buyers should confirm the cure system of the specific grade rather than assume.

Can HCR be platinum-cured?

Yes. HCR can use platinum or peroxide curing systems. The appropriate option depends on processing, performance and application requirements.

Does HCR require post-curing?

Some HCR formulations, particularly selected peroxide-cured products, may require post-curing. Not every HCR component has the same requirement.

Is LSR cheaper than HCR?

LSR may achieve a lower unit cost at high volume because of automation and short cycles, but its initial tooling investment is often higher. HCR can be more economical for simple or lower-volume components.

Which material is better for tight tolerances?

LSR molding can provide excellent repeatability, but silicone remains flexible and requires appropriate measurement methods. HCR can also meet demanding tolerances with good tooling and process control.

Get Instant Quote & Free Samples Now!
Share The Post Now:
Author Ronnie Tang

Hey there, I’m Ronnie Tang!

I love the silicone packaging industry because it allows me to enhance the appearance and appeal of my clients’ products. If you have any questions about silicone bags, please feel free to contact me; I’d be happy to answer them!

You may also find these topics interesting

LSR vs HCR uncured silicone material comparison

LSR vs HCR: A Complete Comparison for Silicone Product Manufacturing

The central difference in the LSR vs HCR comparison is the material’s consistency before curing and the manufacturing system required to process it. Liquid silicone rubber (LSR) is a pumpable,

Silicone types properties and applications guide

Silicone Types Explained: Properties, Differences and Applications

Silicone types can be classified in several ways: by physical form, polymer chemistry, curing mechanism, processing method and intended application. Common terms include liquid silicone rubber (LSR), high-consistency rubber (HCR),

What is silicone material structure and applications

What Is Silicone? Properties, Types, Manufacturing and Applications

What is silicone? Silicone is a family of synthetic polymers built around a backbone of alternating silicon and oxygen atoms, with organic groups attached to the silicon. By adjusting its

Explore latest products

Get Our Full Catalog

*Your email will be kept confidential.